The depolymerization process of the molten input raw material takes place in the depolymerization chamber under low pressure and at a temperature of up to 600° C. The turbine that applies the molten input raw material to the shell of the depolymerization chamber rotates at low speed and is changed every 5 years. A replacement depolymerization turbine is also supplied with the PWED plant. The replaced depolymerization turbine is being repaired and is being prepared for the next replacement.
The molten layer of the input raw material evaporates into a mixture of hydrocarbon gases and enters the process of condensation of diesel and gas fractions.